ABSTRACT

Since its introduction to dentistry more than a decade ago, zirconia ceramic has raised remarkable interest and gained popularity. This is due to its outstanding mechanical properties that permit its use as framework material in the fabrication of fixed dental prostheses, or as dental abutments and implants. The exceptional strength and toughness of zirconia ceramic stems from what is commonly known as stress-induced transformation.

Keywords: Zirconia; Dental crowns; Fixed prosthesis

INTRODUCTION

Zirconia, one of the most promising candidate materials for all-ceramic dental restorations, exists in three crystallographic structures, monoclinic (m), tetragonal (t) and cubic (c). The monoclinic form is stable from room temperature to 1170 oC, then transforms to a tetragonal from 1170 oC to 2370 oC. The structure becomes cubic above 2370 oC and up to melting point1. Upon cooling, the transformation from tetragonal to monoclinic (t-m) is accompanied by an increase in volume (~4.4%) and subsequently leading to shattering upon cooling2, 3. In order to prevent this transformation upon cooling, pure zirconia is alloyed with stabilizing oxides, such as CaO, MgO, Y2O3 or CeO2, to retain the tetragonal form in a metastable state at room temperature (3-5). Yttrium oxide is the most widely used stabilizer in dental zirconia, at a concentration of 3 mol.% (3Y-TZP).

PROPERTIES OF ZIRCONIA

One of the most prominent characteristics of zirconia ceramics is their martensitic stress-induced transformation, where the crystalline structure in solid state is changed through athermal, diffusionless motion of atomic boundaries, which proceeds at the speed of sound4,6,7. The overall mechanism of martensitic transformation is the conversion of tetragonal phase to monoclinic phase caused by shearing displacement of zirconia ions, and the displacement of oxygen ions from tetragonal to monoclinic lattice along the c axis8. The martensitic t-m transformation is induced either by temperature or external stress under isothermal conditions4,9. Both transformations are important, in which temperature-driven transformation will determine the amount of tetragonal phase remaining after thermal cycling, whereas stress-induced transformation will ensure the excellent fracture toughness of zirconia ceramics10.

The stress-induced phase transformation of zirconia ceramics is the process of phase transformation from metastable tetragonal to stable monoclinic in the tensile field around the tip of an advancing crack. This transformation is associated with an increase in volume9, leading to a net compressive stress field at the crack-tip. This stress-induced volumetric change reduces the local crack tip intensity, and increases the resistance of crack propagation with a toughening effect.

USES OF ZIRCONIA

Due to their excellent mechanical properties, zirconia ceramics are not only used in industrial applications, but also in biomedical and dental applications1. A major biomedical application is total hip or knee replacements, with excellent biocompatibility11, 12. The clinical success of zirconia femoral heads led to the implantation of more than 600,000 prostheses worldwide13. Biomedical grade 3Y-TZP exhibits optimal mechanical strength due to the stress-induced phase transformation toughening, as mentioned earlier. However, metastable 3Y-TZP is also susceptible to low temperature degradation (LTD) or aging in the presence of water14, 15 or in vivo. An autocatalytic and progressive t-m transformation at the surface of the prosthesis leads to grain pull out, surface roughening and micro-cracking. The aging process is also associated with wear and may lead to crack propagation and catastrophic failure, as reported for a series of femoral heads in 200113,14.

Metal-free dental restorations are becoming increasingly popular due to their superior esthetics and concerns with potential allergies to metals16. All-ceramic dental restorations are custom-fabricated and are therefore likely to present some processing defects. For example, heat pressing induces the creation of porosity within leucite-based or lithium-disilicate-based restorations. Hard machining introduces residual stresses in leucite-based and lithium-disilicate based ceramics17. This explains why hard machined all-ceramic restorations are limited to single unit or short span multi-unit restorations. Zirconia ceramics were introduced to dentistry in 2001 due to their excellent mechanical properties and acceptable esthetics, allowing their use for the fabrication of posterior fixed partial prostheses. Zirconia ceramics are also used as a core materials with reduced thickness for veneering, or full contour monolithic restorations18.

CLINICAL PERFORMANCE

To date, zirconia dental ceramics have had an excellent track record in terms of clinical performance. Cumulative 5-year survival rates of more than 95% have been reported, with fractures of the veneering porcelain being the most common complication19-21. The mechanism for chipping of the veneering porcelain has been linked to the difference between the coefficient thermal contraction between zirconia and veneering materials, and tempering stresses created during rapid cooling17. Although these issues have been successfully addressed, monolithic zirconia dental restorations are becoming a popular alternative to bilayered zirconia-based dental restorations. Zirconia dental restorations are fabricated through the soft machining process, using computer-aided design/computer-aided manufacture (CAD/CAM). The partially sintered 3 mol.% yttria- stabilized zirconia (3Y-TZP) blocks are milled and sintered at high temperature to achieve full density as recommended by the manufacturers, e.g. BruxZirTM HT 2.0 is sintered at 1580 oC for 2.5 hours22. The sintering temperature determines zirconia grain size, phase assemblage, and mechanical properties. Higher sintering temperatures lead to an increase in grain size, but a decrease in tetragonal content23. Meanwhile, upon the sintering process, the pre-sintered zirconia blocks are subject to dimensional shrinkage ~ 20-25%24. Although the dimensional shrinkage is compensated by the computer-aided design, the restorations often require internal adjustments. In addition, surface adjustments of the restorations are often necessary to achieve optimal occlusion, proper seating and improve bonding by creating micromechanical retentions between the restoration and luting cement. Grinding followed by polishing with polishing kits are recommended for occlusal adjustments 25, whereas air abrasion is performed to improve the mechanical retention between zirconia restorations and luting cements 26- 29. These surface adjustments are likely to trigger the stress-induced phase transformation, which is accompanied by the formation of a compressive stress layer, leading to an increase in mechanical properties30-33. However, these surface adjustments also induce surface and/or subsurface damage34. The efficacy of the phase transformation is dependent on the mean zirconia grain size, where larger grains are more likely to transform to the monoclinic phase14, 17, 35. The mechanical strength of zirconia is also directly dependent on the thickness of compressive stress zone33,36. X-ray diffraction (XRD) analysis also showed that residual stresses created by surface treatments are associated with alterations of the XRD-profile consisting in the following:

  1. Shift in the peak position of the main tetragonal t101 reflection 37,
  2. An increase in the amount of monoclinic volume fraction 33,
  3. An increase in the amount of ferroelastic domain switching 38
  4. An increase in the Full-Width at Half-Maximum of the main tetragonal t101 reflection 39 .

The effect of various surface treatments on the strength of zirconia ceramics has been studied extensively30, 32, 40, 41. It was shown that air abrasion with fine particles was more efficient in promoting the formation of a thick compressive stress layer, and was associated with an increase in mean biaxial flexural strength. Meanwhile, surface modifications created by air abrasion with coarse particles or grinding with diamond coated instruments led to mixed results, either increasing 32,41 or decreasing the mean biaxial flexural strength40,42. Polishing after grinding was shown to decrease the thickness of the compressive stress layer as well as the size of the flaws created by grinding, and consequently associated with a decrease in strength43.

CONCLUSION

Understanding the effect of surface modifications, e.g. grinding, polishing and air- abrasion on the thickness of the compressive stress layer and subsurface damage is critical in the achievement of successful restorations. These modifications are likely to affect the long-term performance of zirconia dental restorations, but to date; assessment of subsurface damage has been limited.

REFERENCES

  1. Piconi C, Macauro G. Zirconia as a ceramic biomaterial. Biomaterials. 1999;20:1- 25.
  2. Subbarao EC. Zirconia-an overview. In: Heuer AH, Hobbs LW, editors. Science and technology of zirconia. 3. Columbus, OH: The American Ceramic Society; 1981. p. 1-24.
  3. Garvie RC, Nicholson PS. Phase analysis in zirconia systems. J Am Ceram Soc. 1972;55(6):303-5.
  4. Garvie RC, Hannink RH, Pascoe RT. Ceramic steel? Nature. 1975;258:703-4.
  5. Heuer AH, Lange FF, Swain MV, Evans AG. Transformation toughening: An overview. J Am Ceram Soc. 1986;69(3):i-iv.
  6. Green DJ, Hannink RH, Swain MV. Transformation toughening of ceramics. 1989.
  7. Kelly PM, Francis Rose LR. The martensitic transformation in ceramics — its role in transformation toughening. Progress in Materials Science. 2002;47(5):463- 557.
  8. Ge QL, Lei TC, Mao JF, Zhou Y. In situ transmission electron microscopy observations of the tetragonal-to-monoclinic phase transformation of zirconia in Al2O3-ZrO2 (2 mol % Y2O3) composite. 819-22 p.
  9. Evans AG, Cannon RM. Overview no. 48: Toughening of brittle solids by martensitic transformations. Acta Metallurgica. 1986;34(5):761-800.
  10. Basu B. Toughening of yttria-stabilised tetragonal zirconia ceramics. International Materials Reviews. 2005;50(4):239-56.
  11. Christel P, Meunier A, Heller M, Torre JP, Peille CN. Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia. Journal of biomedical materials research. 1989;23(1):45-61.
  12. Hulbert SF, Morrison SJ, Klawitter JJ. Tissue reaction to three ceramics of porous and non-porous structures. Journal of biomedical materials research. 1972;6(5):347-74.
  13. Chevalier J, Gremillard L. Ceramics for medical applications: A picture for the next 20 years. Journal of the European Ceramic Society. 2009;29(7):1245-55.
  14. Chevalier J. What future for zirconia as a biomaterial? Biomaterials. 2006;27(4):535-43.
  15. Cattani-Lorente M, Scherrer SS, Ammann P, Jobin M, Wiskott HW. Low temperature degradation of a Y-TZP dental ceramic. Acta biomaterialia. 2011;7(2):858-65.
  16. Denry IL. All-ceramic restorations. In: Rosenstiel SF, editor. Contemporary Fixed Prosthodontics. Saint-Louis, MO: Mosby Elsevier; 2006. p. 777.
  17. Denry I. How and when does fabrication damage adversely affect the clinical performance of ceramic restorations? Dental Materials. 2013;29(1):85-96.
  18. Denry I, Kelly JR. State of the art of zirconia for dental applications. Dental materials : official publication of the Academy of Dental Materials. 2008;24(3):299-307.
  19. Larsson C, Wennerberg A. The clinical success of zirconia-based crowns: a systematic review. The International journal of prosthodontics. 2014;27(1):33-43.
  20. Le M, Papia E, Larsson C. The clinical success of tooth- and implant-supported zirconia-based fixed dental prostheses. A systematic review. J Oral Rehabil. 2015;42(6):467-80.
  21. Molin MK, Karlsson SL. Five-year clinical prospective evaluation of zirconia- based Denzir 3-unit FPDs. The International journal of prosthodontics. 2008;21(3):223-7.
  22. Bruxzir milling blanks instruction for use CA: Glidewell Direct; [Available from: http://www.glidewelldental.com.
  23. Ruiz L, Readey MJ. Effect of heat-treatment on grain size, phase assemblage, and mechanical properties of 3 mol% Y-TZP. J Am Ceram Soc. 1996;79(9):2331-40.
  24. Filser F, Kocher P, Weibel F, Luthy H, Scharer P, Gauckler LJ. Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM). Int J Comput Dent. 2001;4(2):89-106.
  25. Miyazaki T, Nakamura T, Matsumura H, Ban S, Kobayashi T. Current status of zirconia restoration. Journal of prosthodontic research. 2013;57(4):236-61.
  26. Fischer J, Grohmann P, Stawarczyk B. Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites. Dent Mater J. 2008;27(3):448-54.
  27. Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dental materials : official publication of the Academy of Dental Materials. 2007;23(1):45-50.
  28. Laboratories G. Instructions for adjusting and polishing BruxZir crown & bridge [Available from: http://www.bruxzir.com/dental-zirconia/technical-information/.
  29. ESPE M. RelyX luting plus resin modified glass ionomer cement.
  30. Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dental materials : official publication of the Academy of Dental Materials. 1999;15(6):426-33.
  31. Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. Strength and reliability of surface treated Y-TZP dental ceramics. Journal of biomedical materials research. 2000;53(4):304-13.
  32. Denry IL, Holloway JA. Microstructural and crystallographic surface changes after grinding zirconia-based dental ceramics. J Biomed Mater Res B-Appl Biomater. 2006;76B(2):440-8.
  33. Deville S, Chevalier J, Grémillard L. Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia. Biomaterials. 2006;27(10):2186-92.
  34. Chintapalli RK, Marro FG, Jimenez-Pique E, Anglada M. Phase transformation and subsurface damage in 3Y-TZP after sandblasting. Dental materials : official publication of the Academy of Dental Materials. 2013;29(5):566-72.
  35. Chevalier J, Grémillard L, Virkar AV, Clarke DR. The Tetragonal-Monoclinic Transformation in Zirconia: Lessons Learned and Future Trends. J Am Ceram Soc. 2009;92(9):1901-20.
  36. Chevalier J, Olagnon C, Fantozzi G. Subcritical Crack Propagation in 3Y-TZP Ceramics: Static and Cyclic Fatigue. J Am Ceram Soc. 1999;82(11):3129-38.
  37. Noyan IC, Cohen JB. Determination of Strain and Stress Fields by Diffraction Methods. New York, NY: Springer New York; 1987. 117-63 p.
  38. Virkar AV, Matsumoto RLK. Ferroelastic Domain Switching as a Toughening Mechanism in Tetragonal Zirconia. Journal of the American Ceramic Society. 1986;69(10):C-224-C-6.
  39. Garvie RC, Hannink RH, Pascoe RT. Ceramic Steel? Sōmiya S, Moriyoshi Y, editors. Dordrecht: Springer Netherlands; 1990. 253-7 p.
  40. Curtis AR, Wright AJ, Fleming GJP. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. Journal of dentistry. 2006;34(3):195-206.
  41. Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. Journal of dentistry. 2005;33(1):9-18.
  42. Kosmac T, Oblak C, Marion L. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics. J Eur Ceram Soc. 2008;28(5):1085-90.
  43. Guazzato M, Albakry M, Quach L, Swain MV. Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia- reinforced dental ceramic. Dental materials : official publication of the Academy of Dental Materials. 2005;21(5):454-63.

Disclaimer from Guident

The views and opinions expressed in articles published in Guident are solely those of the authors and do not necessarily reflect the views of the editors, the editorial board or the publisher, Ivory India. Guident does not endorse any product, technique or treatment described. Clinical content is intended for qualified dental and medical professionals and is not a substitute for individual clinical judgement. Guident, its editors and the publisher accept no liability for any consequence arising from the use of information published in the journal.

How to cite this article

Dr. Akash Shah Vadodra. Use of Zirconia in Dentistry. Guident. 2018 Aug;11(9). Available from: https://guident.net/articles/general/use-of-zirconia-in-dentistry.html

Related articles

More in General Dentistry/Community Dentistry

All 249 articles
Call for papers

Publish your clinical work in Guident

Original research, case reports and review articles are welcomed from clinicians and researchers worldwide. Every submission is assessed by the editorial board.